Technical data

Type: extra hard, Type 4 according to ISO 1562, only Duceragold ceramic can be fused on
Colour: yellow

Compositions in

weight-%

(atom-%)

Gold/Platin metals

82,9

(68,1)

Gold (Au)

73,8

(60,5)

Platin (Pt)

9,0

(7,5)

Iridium (Ir)

0,1

(0,1)

Silver (Ag)

9,2

(13,8)

Copper (Cu) 

4,4

(11,2)

Zinc (Zn)

2,0

(4,9)

Indium (In) 1,5 (2,1)

 

    europaflagge

Information presented on  this webpage only refers  to European Markets.

Melting range  (°C)   900 - 990
Average linear CTE*   (µm/m× K)   16,7 (25 - 500 °C)   16,8 (25 - 600 °C)
Vickers hardness  (HV 5)   w 150   a 230   b 200
0,2 %-yield strength**  (N/mm2)   a 500   b 480
Tensile strength**  (N/mm2)   a 650   b 630
Elongation  (%)   a 6   b 12

Density (g/cm3)   16,7

* coefficient of thermal expansion
** measurements with samples according to ISO 1562, 9693, 8891
w = soft
a = hardened
b/g = attainable hardness due slow cooling in the mould

Processing instructions (Download)