Degunorm® eco

Technical data

Type: extra hard, Type 4 according to ISO 1562, can be fused on Duceragold ceramic according to ISO 9693
Colour: bright yellow

Compositions in

weight-%

(atom-%)

Gold/Platin metals

70,7

(56,6)

Gold (Au)

59,8 

(45,1)

Platin (Pt) 5,9 (4,5)

Palladium (Pd)

4,9

(6,9)

Iridium (Ir)

0,1

(0,1)

Silver (Ag)

24,3 

(33,5)

Zinc (Zn) 

3,5

(8,0)

Indium (In)

1,5

(1,9)

 

    europaflagge

Information presented on  this webpage only refers  to European Markets.

Melting range  (°C)   970 - 1030 
Average linear CTE* (µm/m× K)   16,6 (25 - 500 °C)   17,1 (25 - 600 °C)
Vickers hardness**  (HV 5)   a 220   b 200
0,2 %-yield strength**  (N/mm2)   a 610   b 600
Tensile strength**  (N/mm2)   a 690   b 680
Elongation**  (%)   a 3   b 5

Density (g/cm3)   14,9

* coefficient of thermal expansion
** measurements with samples according to ISO 1562, 9693, 8891
w = soft
a = hardened